RECOVERY OF GOLD,SILVER AND
PLATINUM GROUP METALS
(IT IS BEST TO RECOVER PLATINUM GROUP METALS IN A CLS ELECTROLITIC TANK) ELECTROLITIC RECOVERY AND REFINING IF YOU NEED SUPPLIES GO TO OUR
STORE ENTER
THE STORE
GOLD CAN BE RECOVERED AND REFINED AT THE SAME TIME IN A ELECTROLITIC BATH OF HYDROCHLORIC (MURATIC) ACID. IT DOES TAKE ALOT OF ELECTRIC POWER,THAT IS THE MAIN REASON IT IS NOT WIDELY USED. HOWEVER A FEW HYBRID SYSTEMS HAVE SURFACED THAT MAKE IT MORE ECONOMICAL. AS A REFINER MYSELF I DO NOT RECOMEND ELECTROLITIC SYSTEMS FOR GOLD ON A SMALL SCALE, THEY ARE HOWEVER VERY WELL SUITED FOR PLATINUM. CLS LEACH TANK. (MATERIALS NEEDED) 5 GALLON PAIL STAINLESS STEEL CATHODE PLATE 3 TO 5 INCHES WIDE (NEGATIVE) GRAPHITE ROD(POSITIVE) MOUNTED ON ONE SIDE OF THE PAIL IS A GRAPHITE ROD,EXTENDING 1-3 INCHES INTO THE LIQUID. THE OTHER SIDE HAS A REMOVABLE STAINLESS STEEL PLATE SUSPENDED INTO THE LIQUID 2-6 INCHES. ATTACH A DC VOLTAGE SOURCE(BATTERY,BATTERY CHARGER,JUMP CABLES,ETC)-/+ AS SHOWN ABOVE. ALL METALS FROM THE RAW MATERIALS PLACED INTO THE LIQUID WILL PRECIPITATE AND COLLECT ON THE STAINLESS STEEL PLATE AS A RED/BROWN MUD(BROWN/BLACK COLOR=HIGH GOLD&PGM'S),,,(RED=ALOT OF COPPER PLUS LEAD,SILVER) CYANIDE LEACH SUBSTITUTE - CLS SYSTEM.(PRIMARILY FOR PLATINUM CATALITIC CORES) FOR SYSTEMS AND SUPPLIES SEE ACTION MINING SERVICES CLS LEACH MIX ADD 1 GALLON WATER TO THE TANK. ADD 1 GALLON MURATIC ACID ADD 100 ml SULFURIC ACID MIX 1 OZ CLS WITH A SMALL AMOUNT OF WATER ADD THE CLS/WATER MIX TO THE TANK SLOWLY. ADD WATER TO COMPENSATE FOR EVAPORATION WITH USE KEEP TEMP BETWEEN 120* -180*F |
||
|